Back pressure porosity can be reduced by:

Correct Answer: Proper or increased burnout temperature and proper casting pressure
Description: Back pressure porosity This is caused by inadequate venting  of the mold. Air is trapped in the mold and is unable to escape. The sprue pattern length should be adjusted so that there is not more than 1/4” thickness of the investment between the bottom of the casting ring and the wax pattern. When the molten metal enters the mold, the air inside is pushed out through the porous investment at the bottom. If the bulk of the investment is too great, the escape of air becomes difficult causing increased pressure in the mold. The gold will then solidify before the mold is completely filled resulting in a porous casting with rounded short margins. Avoided by Using adequate casting force. Use investment of adequate porosity. Place pattern not more than 6 to 8 mm away from the end of the ring. Providing vents in large castings. Proper burnout temperature. Basic Dental Materials by John Manappallil ed 4 pg370
Category: Dental
Share:

Get More
Subject Mock Tests

Practice with over 200,000 questions from various medical subjects and improve your knowledge.

Attempt a mock test now
Mock Exam

Take an exam with 100 random questions selected from all subjects to test your knowledge.

Coming Soon
Get More
Subject Mock Tests

Try practicing mock tests with over 200,000 questions from various medical subjects.

Attempt a mock test now
Mock Exam

Attempt an exam of 100 questions randomly chosen from all subjects.

Coming Soon
WordPress › Error

There has been a critical error on this website.

Learn more about troubleshooting WordPress.